1) Boiling occurs when wet furnace materials are mixed with furnace materials, resulting in uneven outgassing and atomisation of large quantities of furnace materials. Magnesia contains water and can be atomised in the form of a sand pit.
2) The furnace material mixture is not uniform and the melting process is also not uniform.
3) The heat distribution in the unit is inadequate, the reaction is slow and the melting time is excessive. This problem can be attributed to three main factors: insufficient amount of reducing agent, low heat release rate, and low preheating temperature of the furnace material. These factors contribute to the formation of cold shock during the melting process. A significant amount of slag accumulates at the base of the iron ingot, which is accompanied by the presence of iron particles in the slag or lack of melting between the iron ingot and the slag, which is relatively loose or contains slag.
4) Optimising the heat distribution in the unit or the preheating temperature promotes more reactions and more mixing of the slag, which can lead to slag spattering. Iron ingot is characterised by hardness and resistance to fracture, while the aluminium content of iron ingot is high, which may lead to lower production.
Abnormal Phenomena In Ferrotitanium Smelting
Oct 16, 2024
Leave a message